Heatbath/Park Parcure 300 Rubber Cure Salt

Category Ceramic , Fluid , Quenchant
Manufacturer Heatbath Corporation - Park Metallurgical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Heatbath/Park Parcure 300 Rubber Cure Salt.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A nitrite-free alternative for customers concerned with the introduction of nitrosamines from the alkali nitrite raw materials used in the production of commercial rubber cure salts. Within its working range, Parcure 300 exhibits viscosities less than or equal to more conventional salts now used; so resultant dragout could be less.Information provided by Heatbath Corporation - Park Metallurgical.
Thermal Properties Metric English Comments
Melting Point 149 - 163 °C
300 - 325 °F
Maximum Service Temperature, Air 593 °C
1100 °F
Upper limit of working range
Minimum Service Temperature, Air 177 °C
350 °F
Lower limit of working range