Polymer Property : Melting Point = 163 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 159 - 163 °C
318 - 325 °F
Hong Kun Group AO 1790 Antioxidant
Chemical name: 1,3,5-tris(4-tert-butyl-3-hydroxy-2,6-dimethylbenzCAS No. 40601-76-1All information provided by Hongkun Group
Melting Point 149 - 163 °C
300 - 325 °F
Heatbath/Park Parcure 300 Rubber Cure Salt
A nitrite-free alternative for customers concerned with the introduction of nitrosamines from the alkali nitrite raw materials used in the production of commercial rubber cure salts. Within its work..
Melting Point 144 - 163 °C
291 - 325 °F
Indium Corp. Indalloy® 97 Pb-Sn-Bi Solder Alloy
Good general purpose step soldering alloy.Information provided by the manufacturer, Indium Corporation.