Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | 816 °C | 1500 °F | Lower limit of working range |
Heatbath/Park #18 Pack Carburizer A non-burning type compound adapted to direct quenching. Barium containing this compound gives the deepest cases for a given time-temperature cycle.Information provided by Heatbath Corporation - Pa.. |
|||
Minimum Service Temperature, Air | 816 °C | 1500 °F | Lower limit of working range |
Heatbath/Park #3 Granular Charcoal Pack Carburizing Compound Commonly used in the heat treatment of steel as a pack-hardening medium.Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Minimum Service Temperature, Air | 816 °C | 1500 °F | Lower limit of working range |
Heatbath/Park Pack Carburizer BF#21 Barium-free pack carburizing compound provides deep cases without the disposal problems associated with barium-containing wastes.Information provided by Heatbath Corporation - Park Metallurgical. |