Material Notes:
Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A thermal conductivity over 200 W/m K is producible.Range of Application: Switching contacts for high-voltage and medium-voltage, heat sinks for passive thermal management, electrodes for erosive processing.Information provided by H.C. Starck.
Physical Properties Metric English Comments
Density 9.50 - 9.90 g/cc
0.343 - 0.358 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 120 - 160

@Load 62.5 kg
120 - 160

@Load 138 lb
2.5 mm ball
Tensile Strength, Ultimate >= 280 MPa
>= 40600 psi
Modulus of Elasticity 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 8.60 µm/m-°C

@Temperature 20.0 - 100 °C
4.78 µin/in-°F

@Temperature 68.0 - 212 °F
9.20 µm/m-°C

@Temperature 20.0 - 300 °C
5.11 µin/in-°F

@Temperature 68.0 - 572 °F
9.60 µm/m-°C

@Temperature 20.0 - 450 °C
5.33 µin/in-°F

@Temperature 68.0 - 842 °F
Thermal Conductivity >= 200 W/m-K
>= 1390 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 32 - 38 %
32 - 38 %
Molybdenum, Mo 62 - 68 %
62 - 68 %
Electrical Properties Metric English Comments
Volume Resistivity 0.0000040 ohm-cm
0.0000040 ohm-cm