Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.0000040 ohm-cm | 0.0000040 ohm-cm | |
H.C. Starck MoCu 65/35 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
Volume Resistivity | 0.0000040 ohm-cm | 0.0000040 ohm-cm | |
H.C. Starck WCu 70/30 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |