Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gwent Electronic Materials C2060602D1 Membrane Touch Switch Paste

Category Fluid , Metal , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Gwent Electronic Materials Ltd.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gwent Electronic Materials C2060602D1 Membrane Touch Switch Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The ink should be gently stirred before use avoiding introduction of air bubbles. It is a polymer based system for printing on polyester, PVC, etc.Can be used in membrane touch switch applicationsScreen Printing Equipment: semi-automatic, manualScreen Types: stainless steel, polyester, mesh 156 to 230tpiSubstrate: Polyester, PVC, or Ceramic.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 39 - 41 %

@Temperature 130 °C
39 - 41 %

@Temperature 266 °F
Viscosity 4000 - 6000 cP

@Shear Rate 230 1/s,
Temperature 25.0 °C
4000 - 6000 cP

@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C
68.0 °F
sealed container
Electrical Properties Metric English Comments
Surface Resistivity per Square 12 - 25 ohm

@Thickness 0.0250 mm
12 - 25 ohm

@Thickness 0.000984 in
Using a 2300 mesh stainless steel screen
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 80.0 °C
0.167 hour

@Temperature 176 °F
30.0 min

@Temperature 60.0 °C
0.500 hour

@Temperature 140 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Coverage cm2/g 288
Using a 200 mesh stainless steel screen