Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Carbon Fiber Filled
Manufacturer Greene Tweed
Trade Name Orthetek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Orthtek WF components work well as metal replacements due to Orthtek’s high strength, low weight, corrosion resistance, and dimensional stability. Orthtek WF is recommended for applications such as nail guides and retractors where radiolucentcy and autoclaving are required.Applications:Medical Trauma – External fixation and targeting devicesMedical Orthopedic – Reconstructive components, retractors, spine instrumentation and surgical instrumentationInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.54 g/cc
1.54 g/cc
ASTM D792
Water Absorption 0.050 %
0.050 %
at 212°F (100°C); ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Yield 627 MPa
91000 psi
ASTM D3039
Elongation at Break 1.0 %
1.0 %
ASTM D3039
Tensile Modulus 60.0 GPa
8700 ksi
ASTM D3039
Flexural Strength 827 MPa
120000 psi
ASTM D790
Flexural Modulus 48.3 GPa
7000 ksi
ASTM D790
Compressive Strength 572 MPa
83000 psi
ASTM D695
Compressive Modulus 55.2 GPa
8000 ksi
ASTM D695
Descriptive Properties Value Comments
Color Black
Fiber Orientation [0/90]s
Fiber Tow Size 3K
Fiber Volume, % 50