Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 827 MPa | 120000 psi | Transverse Rupture |
Pacific Sintered Materials FN-262-S High Strength Nickel Steel Powdered Metal High strength, good impact resistant material for mechanical components. Excellent hardenability.Equivalent MPIF Specification: FN-0405-35All information provided by Pacific Sintered Metals. |
|||
Flexural Strength | 827 MPa | 120000 psi | ASTM D790 |
Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Ortht.. |
|||
Flexural Strength | 827 MPa | 120000 psi | ASTM D790 |
Greene Tweed WR™ 575 PEEK, Bi-Directional Carbon Fiber Filled WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material i.. |
|||
Flexural Strength | >= 830 MPa | >= 120000 psi | Rigidty. Elastic bending fatigue, Longitudinal |
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Flexural Strength | 829 MPa | 120000 psi | Rigidty. Elastic bending fatigue, Longitudinal |
CLAL-MSX NICLAFOR® 1000 TH3 Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Flexural Strength | >= 830 MPa | >= 120000 psi | Rigidty. Elastic bending fatigue, Longitudinal |
CLAL-MSX NICLAFOR® 1000 THX Quenched/Cold Rolled/Precipitation Heat Treated, Rolled Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Flexural Strength | 827 MPa | 120000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals High Strength Nickel Steel FN-262-S Powdered Metal High strength, Good impact resistant material for mechanical components, Excellent hardenability Equivalent MPIF Specification: FN-0405-35Information Provided by Pacific Sintered Metals, a division.. |