Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 48.3 GPa | 7010 ksi | ASTM D790 |
Quantum Composites HTC-9590 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9590 (127-51-3) is a 12K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristic.. |
|||
Flexural Modulus | 48.3 GPa | 7010 ksi | ASTM D790 |
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9593 (127-51-5) is a 3K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics.. |
|||
Flexural Modulus | 48.3 GPa | 7000 ksi | RT, Dry; ASTM D790 |
Renegade Materials Corporation MVK-16 Polyimide FreeForm™ T650-35-3K-UC309-8HS Carbon Fabric MVK-16 is a low-cost polyimide prepreg system developed for long-term, continuous service temperature at 375 – 450°F. MVK-16 exhibits excellent retention of high-temperature mechanical properties .. |
|||
Flexural Modulus | 48.3 GPa | 7000 ksi | ASTM D790 |
Greene Tweed Orthetek® WF Polyketone, Continuous Woven Carbon Fiber Greene Tweed offers precision-molded thermoplastic components made from our high-performance Orthtek® composite materials for a variety of demanding medical and biotechnology applications. Ortht.. |
|||
Flexural Modulus | 48.3 GPa | 7000 ksi | ASTM D790 |
Greene Tweed WR™ 575 PEEK, Bi-Directional Carbon Fiber Filled WR®575 is a thermoplastic composite consisting of bi-directionally oriented carbon fibers in a PEEK matrix. The excellent wear resistance and the fiber orientation of WR575 makes this material i.. |