Material Notes:
Greene Tweed’s Chemraz® 526, a perfluoroelastomer, offers superior chemical compatibility coupled with explosive decompression resistance, making it the ideal compound for fluid handling equipment exposed to extreme chemical environments. Chemraz 526 has a temperature range from -4°F to 482°F (-20°C to 250°C). With its outstanding explosive decompression resistant capabilities, Chemraz 526 is well suited in a range of applications from pumps and valves to oilfield completion equipment.ED (explosive decompression) is a phenomenon that often occurs when high-pressure gas molecules migrate into an elastomer at a compressed state. When the pressure surrounding the elastomer is suddenly released, the compressed gas inside the elastomer tries to expand and exit the elastomer, thus causing ED. Most elastomers experience severe blistering or cracking when the forces of these expanding gases overcome the strength of the surrounding material. However, Chemraz 526 offers superior explosive decompression properties and the broadest chemical compatibility, e.g., better resistance to sour gas, acids, caustics, hot water and steam.Chemraz 526 is available for use as O-rings, gaskets and many other custom shapes.Applications:PumpsValvesOilfield completion equipmentCompressorsInformation provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 1.92 g/cc
1.92 g/cc
ASTM D297
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength at Break 17.8 MPa
2580 psi
ASTM D1414
Elongation at Break 100 %
100 %
ASTM D1414
Tensile Modulus 0.00396 GPa
0.575 ksi
@10% Elongation; ASTM D1414
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Descriptive Properties Value Comments
Color Black