Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.00396 GPa | 0.575 ksi | @10% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 526 Perfluoroelastomer Greene Tweed’s Chemraz® 526, a perfluoroelastomer, offers superior chemical compatibility coupled with explosive decompression resistance, making it the ideal compound for fluid handling equ.. |