Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 2.60 W/m-K @Temperature 100 °C |
18.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 85 K Dense Refractory Brick Description: Corundum based bricks with a mullite bond. Application: rotating incinerator furnacesRemarks: This data represents average values, obtained from samples that were cut from standard bric.. |
|||
Thermal Conductivity | 2.60 W/m-K @Temperature 100 °C |
18.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 90 Dense Refractory Brick Description: This brick can be used in very severe conditions, i.e. in reducing atmosphere at a high temperatures, e.g. in carbon-black furnaces.Remarks: This data represents average values, obtaine.. |
|||
Thermal Conductivity | 2.60 W/m-K @Temperature 100 °C |
18.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 85 KP Dense Refractory Brick Description: This corundum based phosphate bond brick is characterized by a very low porosity, high slag resistance and high strength. Application: rotating incinerator furnaces.Remarks: This data r.. |
|||
Thermal Conductivity | 2.60 W/m-K @Temperature 100 °C |
18.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 85 M Dense Refractory Brick Description: A bauxite based brick with a mullite bond. Application: torpedo ladles, electric arc furnace roofs, cement kilns.Remarks: This data represents average values, obtained from samples that.. |
|||
Thermal Conductivity | 2.60 W/m-K @Temperature 100 °C |
18.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast AK 86 A Dense Refractory Brick Description: This bauxite based brick has a high strength and good erosion resistance. Application in torpedo ladles for the steel industry and outlet zone rotary cement kilns.Remarks: This data rep.. |