Goodfellow Nickel Silver (Cu45/Zn43/Ni10/Pb2)

Category Metal , Nonferrous Metal , Copper Alloy
Manufacturer Goodfellow
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Nickel Silver (Cu45/Zn43/Ni10/Pb2).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available as rod.
Mechanical Properties Metric English Comments
Tensile Strength 460 MPa
66700 psi
Elongation at Break <= 8 %
<= 8 %
Component Elements Properties Metric English Comments
Copper, Cu 45 %
45 %
Lead, Pb 2 %
2 %
Nickel, Ni 10 %
10 %
Zinc, Zn 43 %
43 %