Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 7.28 g/cc
0.263 lb/in³
Mechanical Properties Metric English Comments
Vickers Microhardness 900
900
kg(f)/mm²
Tensile Strength at Break 1500 MPa
218000 psi
Thermal Properties Metric English Comments
Crystallization Temperature 515 °C
959 °F
Maximum Service Temperature, Air 150 °C
302 °F
Component Elements Properties Metric English Comments
Boron, B 16 %
16 %
Iron, Fe 79 %
79 %
Silicon, Si 5.0 %
5.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000125 ohm-cm
0.000125 ohm-cm
Magnetic Coercive Force, Hc 0.20 Oe
0.20 Oe
Magnetic Saturation Flux Density, Bmax 15800 Gauss
15800 Gauss
Magnetic Remanence, Br 0.19 Gauss
0.19 Gauss
Remanence Ratio, B<sub>r</sub>/B<sub>s</sub>
Curie Temperature 405 °C
761 °F
Descriptive Properties Value Comments
Saturation magnetostriction (x10^-6) 27