Polymer Property : Magnetic Remanence, Br = 0.19 Gauss
Polymer Property :
Magnetic Remanence, Br =
0.19 Gauss
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Magnetic Remanence, Br
0.19
Gauss
0.19
Gauss
Remanence Ratio, B<sub>r</sub>/B<sub>s</sub>
Goodfellow Iron 79/Boron 16/Silicon 5 Alloy
Information provided by Goodfellow.