Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Garlock 9122 Nitrile Sheet Rubber Gasketing

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Garlock Rubber Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Garlock 9122 Nitrile Sheet Rubber Gasketing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nitrile (NBR)Superior resistance to aliphatic hydrocarbons, such as oil, fuels, and many types of solvents.Information provided by Garlock Rubber Technologies
Mechanical Properties Metric English Comments
Hardness, Shore A 55 - 65
55 - 65
ASTM D 2240
Tensile Strength 13.8 MPa
2000 psi
ASTM F152
Elongation at Break >= 500 %
>= 500 %
ASTM D 395
Compression Set <= 20 %

@Temperature 100 °C,
Time 79200 sec
<= 20 %

@Temperature 212 °F,
Time 22.0 hour
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C

@Pressure 1.72 MPa
250 °F

@Pressure 250 psi
Minimum Service Temperature, Air -28.9 °C
-20.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 0.157 kV/mm

@Thickness 3.17 mm
4.00 kV/in

@Thickness 0.125 in
Unconditioned; ASTM D149
Descriptive Properties Value Comments
Color Black
Copyright © lookpolymers.com All Rights Reserved