Material Notes:
ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transparency. These products can be injection molded, blow molded, and extruded.Information provided by Greater Eastern Resins Industrial Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength 38.0 MPa
5510 psi
ASTM D412
Tensile Strength, Yield 8.30 MPa

@Strain 50.0 %
1200 psi

@Strain 50.0 %
ASTM D412
9.70 MPa

@Strain 100 %
1410 psi

@Strain 100 %
ASTM D412
21.0 MPa

@Strain 300 %
3050 psi

@Strain 300 %
ASTM D412
Elongation at Break 500 %
500 %
ASTM D412
Tear Strength 100 kN/m
571 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 60
60
ASTM D1044(Taber) H-22
Compression Set 30 %

@Temperature 23.0 °C,
Time 79200 sec
30 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
75 %

@Temperature 70.0 °C,
Time 79200 sec
75 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395