Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 9.70 MPa @Strain 100 % |
1410 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1095AE Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp.. |
|||
Tensile Strength, Yield | 9.70 MPa @Strain 100 % |
1410 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1195A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 9.70 MPa @Strain 50.0 % |
1410 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1198A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 9.70 MPa @Strain 100 % |
1410 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 2090A Poly(caprolactone)ester TPUÂ Resin ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi.. |
|||
Tensile Strength, Yield | 9.70 MPa @Strain 100 % |
1410 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 1090A Poly(adipate)ester TPUÂ Resin ISOTHANE 1000 series products are general purpose poly(adipate)ester based thermoplastic polyurethanes. They exhibit excellent toughness, abrasive resistance, and solvent resistance. These products .. |
|||
Tensile Strength, Yield | 9.70 MPa @Strain 100 % |
1410 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 690A15N Polyester Type Polyurethane Elastomer This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes.. |