Mechanical Properties Metric English Comments
Tensile Strength, Yield 8.30 MPa

@Strain 50.0 %
1200 psi

@Strain 50.0 %
ASTM D412
GRECO ISOTHANE 1095AE Poly(adipate)ester TPU Resin
ISOTHANE 1000 series products are Poly(adipate)ester based thermoplastic polyurethanes with good balanced qualities. They exhibit good toughness, abrasive resistance, solvent resistance, and transp..
Tensile Strength, Yield 8.30 MPa

@Strain 100 %
1200 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 3090AF Polyether TPU Resin
ISOTHANE 3000F Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These pro..
Tensile Strength, Yield 8.30 MPa

@Strain 100 %
1200 psi

@Strain 100 %
ASTM D412
GRECO ISOTHANE 5090A Polyether TPU Resin
ISOTHANE 5000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent bio-compatibility, hydrolytic resistance, fungus resistance, and low temperature performance pro..
Tensile Strength, Yield 8.30 MPa

@Strain 300 %
1200 psi

@Strain 300 %
ASTM D412
GRECO ISOTHANE 2075A Poly(caprolactone)ester TPU Resin
ISOTHANE 2000 series products are polyester poly(caprolactone)ester based thermoplastic polyurethane. They exhibit excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stabi..
Tensile Strength, Yield 8.27 MPa

@Strain 300 %
1200 psi

@Strain 300 %
ASTM D412
Teknor Apex Laripur® LPR 7560EG Thermoplastic Polyurethane
Features: - Excellent performance under extreme and aggressive environments - Superior abrasion and cut resistance - Resistance to chemical, microbial attack and hydrolysis - Excellent flexibility a..
Tensile Strength, Yield 8.27 MPa

@Temperature 21.1 °C
1200 psi

@Temperature 70.0 °F
Flatwise Tensile, Cured at 250°C for 60 min at 30 psi MMM-A-132 and MIL-A-25463.
Hexcel® Redux® 382H (0.06 psf) Film Adhesive
Redux 382H is a 250°F curing modified epoxy film adhesive available in both supported and unsupported versions. Redux 382H is a versatile adhesive system suitable for bonding a wide variety of subs..
Tensile Strength, Yield 8.30 MPa

@Strain 300 %
1200 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® 1175AW Polyether Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes...
Tensile Strength, Yield 8.30 MPa

@Strain 300 %
1200 psi

@Strain 300 %
ASTM D-412
BASF Elastollan® S80A Polyester Type Polyurethane Elastomer
Processed by extrusion or injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fue..