Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fujipoly Industries WSC Connector

Category Polymer , Thermoset , Silicone
Manufacturer Fujipoly Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fujipoly Industries WSC Connector.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fujipoly W connector is capable of connecting fine pitch linear pads and pad grid arrays. It is conductive only in the thickness direction which makes it appropriate for low profile "z-axis" connectionsInformation provided by Fujipoly Industries
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Electrical Properties Metric English Comments
Surface Resistance 1.00e+10 ohm
1.00e+10 ohm
C-Pattern; P = 0.35
Descriptive Properties Value Comments
Current Carrying Capacity 500 mA/mm^2
More than 1,500 hours