Material Notes:
Sarcon GR-L is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and make reliable and complete physical contact.Information provided by Fujipoly Industries
Physical Properties Metric English Comments
Specific Gravity 2.70 g/cc
2.70 g/cc
JIS-K-6220; ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore OO 53
53
SRIS0101; ASTM D-2240
Tensile Strength, Yield 0.200 MPa
29.0 psi
JIS-K-6251(#2)/ASTM D-412
Elongation at Yield 64 %
64 %
JIS-K-6251(#2)/ASTM D-412
Tear Strength 1.00 kN/m
5.71 pli
JIS-K-6252 (Angle)/ASTM D-624
Thermal Properties Metric English Comments
Thermal Conductivity 2.80 W/m-K
19.4 BTU-in/hr-ft²-°F
JIS-R-2618; ASTM D2326
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 2.50e+12 ohm-cm
2.50e+12 ohm-cm
JIS-K-6249/ASTM D257
Dielectric Strength 13.0 kV/mm
330 kV/in
JIS-K-6249; ASTM D-149
Dielectric Breakdown 7000 V
7000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Descriptive Properties Value Comments
Color Grey