Polymer Property : Dielectric Breakdown = 7000 V Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Dielectric Breakdown 7000 V
7000 V
Withstand Voltage [V/min]; AC 60 Hz
Fujipoly Industries Sarcon® 30GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Breakdown 7000 V
7000 V
Withstand Voltage [V/min]; AC 60 Hz
Fujipoly Industries Sarcon® 30Q Thin-Film QR
Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov..
Dielectric Breakdown 7000 V
7000 V
Withstand Voltage [V/min]; AC 60 Hz
Fujipoly Industries Sarcon® 30T Thin-Film TR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Breakdown 7000 V
7000 V
Withstand Voltage [V/min]; AC 60 Hz
Fujipoly Industries Sarcon® 45GSR Thin-Film GSR
Sarcon GSR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GSR is a composite of..
Dielectric Breakdown 7000 V
7000 V
Withstand Voltage [V/min]; AC 60 Hz
Fujipoly Industries Sarcon® 45H Thin-Film HR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Dielectric Breakdown 7000 V
7000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® GR-k Gap Filler Pad
Sarcon GR-k is a general type of thermal conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and mak..
Dielectric Breakdown 7000 V
7000 V
Withstand Voltage [V/min]; JIS-K-6249; ASTM D-149
Fujipoly Industries Sarcon® GR-L Gap Filler Pad
Sarcon GR-L is a highly formable, thermally conductive gel material (no electicity conductive) in a versatile sheet form that easily fits and adheres to most all shapes and sizes of components, and ..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® 23816 Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape
Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal ..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® 2975-8R Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape
Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal ..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® K102 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® K103 Polyimide Film Backing Acrylic Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® M783 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® M832 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® M852 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® M887 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® M98 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® M99 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® SG03-14(R) Premium Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® SG05-14(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® SG06-14(R) Premium Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® 2042-2 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® K250 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® K290ESD Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit ..
Dielectric Breakdown 7000 V
7000 V
1/4" electrode 500 V/sec 25°C in air; ASTM D149
DuPont Teijin Films Melinex® SWC Polyester Film, 92 Gauge
A narrow width film with consistently good handling properties; transparent in thin gauges, slightly hazy in thick gauges, ideally suited for wire and cable wrapping and insulation.Information provi..
Dielectric Breakdown 7000 V
7000 V
Saint-Gobain CHR® M57 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape
Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa..