Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Formosa Plastics Formolene® 2520N Injection Molding Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolene® 2520N Injection Molding Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact Copolymer for Injection MoldingFormolene® 2520N is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional stability. The improved stiffness and impact balance also provides for utility in industrial applications including bins and crates, and small appliances. Formolene® 2520N meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles and components of articles intended for direct food contact. For additional information on approved conditions of use for food contact applications, please refer to the “Products” section on our web site (http://www.fpcusa.com/ourproducts.html).Specimens were injection molded according to the conditions specified in ASTM D4101.Information provided by Formosa Plastics Corporation, USA.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min

@Temperature 230 °C
20 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
2" (50mm) per min.; ASTM D638
Elongation at Yield 6.0 %
6.0 %
2" (50mm) per min.; ASTM D638
Flexural Modulus 1.21 GPa
175 ksi
1.3mm per min, 1% secant; ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved