Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills 43S2A Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Blow Molding Grade , Polypropylene, Film Grade
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills 43S2A Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good clarity.Applications: Film extrusion and blow moldingInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 1.9 g/10 min
1.9 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ASTM D785
Tensile Strength, Yield 26.2 MPa
3800 psi
ASTM D638
Elongation at Yield 14 %
14 %
ASTM D638
Flexural Modulus, 1% Secant 835 MPa
121000 psi
ASTM D790
Tangent Modulus 869 MPa
126000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C
174 °F
ASTM D648
Users viewing this material also viewed the following: