Fiberfil® M-2501 BK Nylon 66, 40% mineral Filled, post industrial

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer FiberFil
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fiberfil® M-2501 BK Nylon 66, 40% mineral Filled, post industrial.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by FIBERFIL Engineered Plastics
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 93.996 MPa
13633 psi
ASTM D638
Flexural Modulus 6.300 GPa
913.7 ksi
Secant; ASTM D790
Izod Impact, Notched 0.352 J/cm

@Thickness 3.17 mm
0.660 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ASTM D648