Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil PP9122 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP9122 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A random copolymer resin designed for extrusion blow molding applications and thermoforming of medical and other specialty devices and packaging. It has excellent organoleptics and very low ash metal content.Availability: North America Features:Autoclave SterilizableClean/High PurityEthylene Oxide SterilizableLow ExtractablesLow to No OdorSteam SterilizableUses: CapsClosuresLabwareMedical PackagingMedical/Healthcare ApplicationsPackagingProcessing Method: Blow Molding, Extrusion, Extrusion Blow Molding, Injection Blow Molding, Profile Extrusion, Sheet Extrusion and ThermoformingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ExxonMobil Method
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.5 MPa
4140 psi
2.0 in/min; ASTM D638
Elongation at Yield 13 %
13 %
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 972 MPa
141000 psi
0.05 in/min; ASTM D790A
1140 MPa
166000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.7 °C
179 °F
ASTM D648
Users viewing this material also viewed the following: