Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 1140 MPa | 166000 psi | 0.5 in/min; ASTM D790B |
ExxonMobil PP9122 Polypropylene Homopolymer Product Description: A random copolymer resin designed for extrusion blow molding applications and thermoforming of medical and other specialty devices and packaging. It has excellent organoleptics.. |