Material Notes:
Product Description: Medium melt flow rate homopolymer. Particularly suitable for general purpose injection moldingAvailability: North America Features:Autoclave SterilizableEthylene Oxide SterilizableGeneral PurposeHigh FlowHigh IsotacticSteam SterilizableUses: Automotive ApplicationsCast FilmCompoundingConsumer ApplicationsMedical/Healthcare ApplicationsPackagingProcessing Method: Injection MoldingInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.3 MPa
5120 psi
2 in/min; ASTM D638
Flexural Modulus, 1% Secant 1530 MPa
222000 psi
0.05 in/min; ASTM D790A
1740 MPa
252000 psi
0.5 in/min; ASTM D790B
Izod Impact, Notched 0.283 J/cm
0.530 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 190 - 218 °C
374 - 424 °F
Typical