Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission Rate | 0.101 cc/m²/day @Temperature 23.0 °C |
0.00650 cc/100 in²/day @Temperature 73.4 °F |
ExxonMobil Method |
ExxonMobil Metallyte™ 18MM882 OPP Film Product Description: An ultra high barrier (UHB), biaxially oriented, multilayer polypropylene film. In addition to an excellent water vapor barrier, this film has an exceptional barrier to oxygen, .. |
|||
Oxygen Transmission Rate | 0.101 cc/m²/day @Temperature 23.0 °C |
0.00650 cc/100 in²/day @Temperature 73.4 °F |
ExxonMobil Method |
ExxonMobil Metallyte™ 18MM883 OPP Film Product Description: An ultra high barrier (UHB), biaxially oriented multilayer polypropylene film. This film has an exceptional barrier to oxygen, flavors and aromas and has an excellent water vapo.. |
|||
Oxygen Transmission Rate | 0.101 cc/m²/day @Temperature 23.0 °C |
0.00650 cc/100 in²/day @Temperature 73.4 °F |
0% RH; ExxonMobil Method |
ExxonMobil Metallyte™ UHB 35MU842 OPP Film Product Description: A metalized high opacity white oriented polypropylene film. It is biaxially oriented, multi-layer polypropylene film with aluminum deposited on an adhesion promoting layer. The .. |