ExxonMobil Exxtral™ MDK310 Performance Polyolefin

Category Polymer , Thermoplastic , Ethylene Butyl Acrylate
Manufacturer Exxon Chemical
Trade Name Exxtral™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Exxtral™ MDK310 Performance Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A medium melt flow rate, 20% mineral-filled polyolefin resin suitable for injection molded consumer products and appliance applications requiring long-term heat ageing resistance. UL continuous service rating of 115°CAvailability: Asia Pacific and North America Features:Detergent ResistantFilledGood Thermal Aging ResistanceHigh Heat ResistanceHigh StiffnessImpact Modified Uses: Appliance ComponentsAppliances Consumer ApplicationsProcessing Method: Injection MoldingInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1900 MPa
275000 psi
0.05 in/min; ASTM D790A
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256A
Gardner Impact 8.84 J

@Thickness 3.17 mm,
Temperature -28.9 °C
6.52 ft-lb

@Thickness 0.125 in,
Temperature -20.0 °F
Geometry GC; ASTM D5420
23.8 J

@Thickness 3.17 mm,
Temperature 22.8 °C
17.6 ft-lb

@Thickness 0.125 in,
Temperature 73.0 °F
Geometry GC; ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 59.4 °C
139 °F
ASTM D648