Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 59.4 °C @Thickness 3.18 mm |
139 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 161J-1-3V/2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 59.4 °C @Thickness 3.18 mm |
139 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 2188GC Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 59.4 °C @Thickness 3.18 mm |
139 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 2188GC-1V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 59.4 °C @Thickness 3.18 mm |
139 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 2188GC-3V Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 59.4 °C @Thickness 3.18 mm |
139 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Packaging 2188NT Polyvinyl Chloride, Rigid (PVC, Rigid) A transparent natural PVC bottle compound for blow molding applications.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 59.4 - 87.8 °C | 139 - 190 °F | Average value: 71.9 °C Grade Count:45 |
Overview of materials for PVC, High Impact This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 59.4 °C | 139 °F | unannealed; ASTM D-648 |
Axiall LSS-8200 Rigid PVC, Extrusion Georgia Gulf LSS-8200 is a special purpose rigid PVC sheet extrusion compound designated for reduced smoke emission properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 59.4 °C | 139 °F | ASTM D648 |
ExxonMobil Exxtral™ MDK310 Performance Polyolefin Product Description: A medium melt flow rate, 20% mineral-filled polyolefin resin suitable for injection molded consumer products and appliance applications requiring long-term heat ageing resistanc.. |