ExxonMobil Escorene™ UL 04331EL Ethylene Vinyl Acetate Copolymer

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 04331EL Ethylene Vinyl Acetate Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 04331EL is a HEVA grade, especially designed for photovoltaic cells and encapsulation applications, requiring a good balance of adhesion and COF. It offers excellent light transmission characteristics. UL 04331EL contains and additive packaging to improve pellet flowability and handling.Availability: Africa & Middle East, Latin America, Europe, North America and South America Applications:EncapsulationHot Melt AdhesivesPhotovoltaic CellsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ExxonMobil method
Vinyl Acetate Content 31.4 %
31.4 %
ExxonMobil method
Melt Flow 43 g/10 min

@Load 2.16 kg,
Temperature 190 °C
43 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 66

@Time 15.0 sec
66

@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 13

@Time 15.0 sec
13

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 6.00 MPa
870 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Tensile Modulus 0.00827 GPa
1.20 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point <= 139 °C
<= 282 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 33.9 °C
93.0 °F
ASTM D1525