Vicat Softening Point 33.9 °C
93.0 °F
ASTM D1525
ExxonMobil Escorene™ UL 04331EL Ethylene Vinyl Acetate Copolymer
Product Description: UL 04331EL is a HEVA grade, especially designed for photovoltaic cells and encapsulation applications, requiring a good balance of adhesion and COF. It offers excellent light tr..