Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Break, TD | 35.9 MPa | 5210 psi | ASTM D882 |
DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Film Tensile Strength at Break, TD | 35.9 MPa | 5200 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00014 is a copolymer of ethylene and vinyl acetate. For film requiring very high toughness, low creep, excellent optical properties and low gel.Availability: Africa & Middle .. |
|||
Film Tensile Strength at Break, TD | 35.9 MPa | 5200 psi | ASTM D882 |
ExxonMobil Escorene™ UL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00014 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
Film Tensile Strength at Break, TD | 35.9 MPa | 5210 psi | ASTM D882 |
Dow DOWLEX™ 2247G Polyethylene Resin Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap.. |
|||
Film Tensile Strength at Break, TD | 35.9 MPa | 5200 psi | ASTM D882 |
Dow ELITE™ 5220G Enhanced Polyethylene Resin High impact and puncture resistance Excellent on-pallet load elongation for higher yields on regular loads Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Film Tensile Strength at Break, TD | 35.9 MPa | 5200 psi | ASTM D882 |
Dow ELITE™ 5230G Enhanced Polyethylene Resin ™ 5230G is produced via INSITE™ Technology from Dow Plastics. It offers high impact strength and good puncture resistance at moderate stretch levels for irregularly shaped loads. In addition, th.. |
|||
Film Tensile Strength at Break, TD | 35.9 MPa | 5210 psi | |
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |