Material Notes:
Strontium Borosilicate glasses have the low refractive indices (1.500). They also have a low coefficient of thermal expansion. CAS # 65997-17-3.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Density 2.44 g/cc
0.0882 lb/in³
Particle Size 12.5 µm
12.5 µm
median
Thermal Properties Metric English Comments
CTE, linear 3.30 µm/m-°C
1.83 µin/in-°F
Optical Properties Metric English Comments
Refractive Index 1.50
1.50
Component Elements Properties Metric English Comments
BaO 14 %
14 %
SiO2 57 %
57 %
Descriptive Properties Value Comments
SrO (%) 14