Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.44 g/cc @Temperature 25.0 °C |
0.0882 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8660 Borosilicate Glass Borosilicate glass for sealing to tungsten, of high cesium content Red eye reduction flash for electronic flashbulbs, longer life in comparison with glass 8487 The heavy metal content for the elem.. |
|||
Density | 2.44 g/cc | 0.0882 lb/in³ | |
Schott NG3 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG1, NG4, NG5, NG9, NG10, NG11, NG 12 |
|||
Density | 2.44 g/cc | 0.0882 lb/in³ | |
Schott NG9 Neutral Density Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG1, NG10, NG11, NG 12 |
|||
Density | 2.44 g/cc | 0.0882 lb/in³ | |
Von Roll Isola IMI MICA MAT® Inorganic Bonded Mica Plate Data provided by Von Roll Isola USA.Rigid plate designed for use as a non-conducting structural component up to 760°C. 100% inorganic so it maintains good physical and electrical properties at ele.. |
|||
Density | 2.44 g/cc | 0.0882 lb/in³ | |
Corning Large Cover Gorilla® Glass Touch Screen Glass Corning® Gorilla® Glass is a damage-resistant cover glass that is elegant, lightweight, and durable enough to resist many real-world events that commonly cause glass failure. The composition of C.. |
|||
Density | 2.44 g/cc | 0.0882 lb/in³ | |
Esstech V-124-1110 Strontium Borosilicate Glass Strontium Borosilicate glasses have the low refractive indices (1.500). They also have a low coefficient of thermal expansion. CAS # 65997-17-4.Information provided by ESSTECH, Inc. |
|||
Density | 2.44 g/cc | 0.0882 lb/in³ | |
Esstech V-124-1125 Strontium Borosilicate Glass Strontium Borosilicate glasses have the low refractive indices (1.500). They also have a low coefficient of thermal expansion. CAS # 65997-17-3.Information provided by ESSTECH, Inc. |