Physical Properties Metric English Comments
Density 2.44 g/cc

@Temperature 25.0 °C
0.0882 lb/in³

@Temperature 77.0 °F
Schott Glass 8660 Borosilicate Glass
Borosilicate glass for sealing to tungsten, of high cesium content Red eye reduction flash for electronic flashbulbs, longer life in comparison with glass 8487 The heavy metal content for the elem..
Density 2.44 g/cc
0.0882 lb/in³
Schott NG3 Neutral Density Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG1, NG4, NG5, NG9, NG10, NG11, NG 12
Density 2.44 g/cc
0.0882 lb/in³
Schott NG9 Neutral Density Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz..Similar glasses include NG3, NG4, NG5, NG1, NG10, NG11, NG 12
Density 2.44 g/cc
0.0882 lb/in³
Von Roll Isola IMI MICA MAT® Inorganic Bonded Mica Plate
Data provided by Von Roll Isola USA.Rigid plate designed for use as a non-conducting structural component up to 760°C. 100% inorganic so it maintains good physical and electrical properties at ele..
Density 2.44 g/cc
0.0882 lb/in³
Corning Large Cover Gorilla® Glass Touch Screen Glass
Corning® Gorilla® Glass is a damage-resistant cover glass that is elegant, lightweight, and durable enough to resist many real-world events that commonly cause glass failure. The composition of C..
Density 2.44 g/cc
0.0882 lb/in³
Esstech V-124-1110 Strontium Borosilicate Glass
Strontium Borosilicate glasses have the low refractive indices (1.500). They also have a low coefficient of thermal expansion. CAS # 65997-17-4.Information provided by ESSTECH, Inc.
Density 2.44 g/cc
0.0882 lb/in³
Esstech V-124-1125 Strontium Borosilicate Glass
Strontium Borosilicate glasses have the low refractive indices (1.500). They also have a low coefficient of thermal expansion. CAS # 65997-17-3.Information provided by ESSTECH, Inc.