Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Entec Hypel® PELD2/.920 LDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Molded
Manufacturer Entec Engineered Resins
Trade Name Hypel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Entec Hypel® PELD2/.920 LDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 13.6 MPa
1970 psi
ASTM D638
Elongation at Break 600 %
600 %
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 90.0 °C
194 °F
Rate A, Loading 1 (10 N); ASTM D1525