Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
Manufacturer Ensinger
Trade Name Tecatron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecatron® XP-86 Compression Molded PPS Compound, with 40% Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run production and yields products which are homogenous with low process stress.TECATRON PPS is a highly crystalline high-temperature thermoplastic with an excellent balance of cost, temperature resistance, strength, chemical resistance and flame retardance. TECATRON PPS is often used when long-term high-temperature performance and dimensional stability are a must, even in the presence of aggressive chemicals.Applications:Fuel InjectorsManifoldsPumpsPistonsGearsV-Packing GasketsBearingsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.51 g/cc
0.0546 lb/in³
ASTM D792
Filler Content 40 %
40 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 99
99
ASTM D785
Tensile Strength 77.2 MPa
11200 psi
ASTM D638
Elongation at Break 1.1 %
1.1 %
ASTM D638
1.2 %
1.2 %
Flexural Strain; ASTM D790
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Flexural Strength 126 MPa
18300 psi
ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Compressive Strength 169 MPa
24500 psi
10% Deformation; ASTM D695
Compressive Modulus 4.83 GPa
700 ksi
ASTM D695
Izod Impact, Notched 0.278 J/cm
0.520 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Color Black