Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eastman Heatwave CF746 Polymer  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eastman Heatwave CF746 Polymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 inch) cubical shaped. This non-extractable UV inhibitor absorbs damaging wavelengths of light, protecting the contents of the package. Heatwave has unique features that enable blow molding exceptionally thermally stable containers for the hotfill industry. Developed for food-contact containers, Heatwave polymer meets applicable FDA regulations for hot-fill containers.Applications/UsesBottlesFood PackagingHot-fill containers
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Crystalline Density; ASTM D1505
Melt Density 1.20 g/cc

@Temperature 285 °C
0.0434 lb/in³

@Temperature 545 °F
ASTM D1238
Viscosity Measurement 0.78 - 0.82
0.78 - 0.82
Intrinsic; VGAS-A-AN-G-V-1
Thermal Properties Metric English Comments
Heat of Fusion 67.0 J/g
28.8 BTU/lb
ASTM E793
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
DSC
1.40 J/g-°C

@Temperature 80.0 °C
0.335 BTU/lb-°F

@Temperature 176 °F
DSC
1.50 J/g-°C

@Temperature 100 °C
0.359 BTU/lb-°F

@Temperature 212 °F
DSC
1.80 J/g-°C

@Temperature 200 °C
0.430 BTU/lb-°F

@Temperature 392 °F
DSC
2.00 J/g-°C

@Temperature 280 °C
0.478 BTU/lb-°F

@Temperature 536 °F
DSC
Melting Point 246 °C
475 °F
Crystalline Peak Melting Point; ASTM D3418
Optical Properties Metric English Comments
UV Transmittance <= 10 %

@Thickness 0.305 mm,
Wavelength 370 nm
<= 10 %

@Thickness 0.0120 in,
Wavelength 370 nm
oriented film; VCSC-A-AN-G-UV-5
Descriptive Properties Value Comments
Acetaldehyde <3ppm
VKCA-A-AS-G-GC-001
Color, CIE a* -1.9 ± 1.5
VGAS-A-AN-G-RS-001
Color, CIE b* -1.1 ± 1.5
VGAS-A-AN-G-RS-001
Color, CIE L* >72.5
VGAS-A-AN-G-RS-001
Fines, wt%, max 0.5
VGAS-A-AN-G-GA-1
Users viewing this material also viewed the following: