Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
Polycasa XT 620 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
Polycasa XT 630 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
Polycasa XT 610 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Plaskolite Optix® PL-76 Acrylic Resin
(discontinued **) Injection/extrusion pellets. Medium heat resistance with higher flow than PL-52 pellets.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Plaskolite Optix® PL-200 Acrylic Resin
(discontinued **) Injection molding grade pellets.Data provided by the manufacturer, Plaskolite, Inc. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | DSC |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | Average value: 1.50 J/g-°C Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Specific Heat Capacity | 1.50 - 1.90 J/g-°C | 0.359 - 0.454 BTU/lb-°F | Average value: 1.80 J/g-°C Grade Count:5 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | Average value: 1.58 J/g-°C Grade Count:6 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
Specific Heat Capacity | 1.50 - 1.60 J/g-°C | 0.359 - 0.382 BTU/lb-°F | DSC |
Wacker Silicones Geniomer® 200 Silicone TPE Elastomer SLM TPSE 200 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | DIN 52612 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction .. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Hippe PA 6 Nylon 6 Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Hippe PA 66 GF 30 Nylon 66 30% Glass fiber Reinforced These polyamide components being reinforced with glass fiber up to 30% are not only highly wear-resistant, but also show high mechanical strength, stiffness and dimensional stability. They can also.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
Hippe PBT GF 30 Polybutylene Terephthalate 30% Glass fiber Reinforced PBT GF is a highly versatile, semi-crystalline structural thermoplastic reinforced with 30% glass fiber, with very high rigidity and strength characteristics and excellent electrical insulation prop.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | Melt |
Covestro Makrolon® DP1-1888* Polycarbonate, 20% Glass Filled ISO 7391-PC,MR,(,,)-09-3,GF20Developmental productMVR (300 °C/1.2 kg) 10 cm3/10 min20 % Glass fiber reinforcedMilled fiberMedium viscosityEasy releasegood surface qualityInjection molding - Melt te.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry) Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur B 4500 PBT Ultradur B4500 is a general-purpose injection molding grade for high-precision, high-toughness, and dimensionally stable engineering parts. It conforms to FDA requirements of 21 CFR 177.1660. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur S 4090 G6 30% Glass Filled PBT Ultradur S 4090 G6 is a 30% glass reinforced PBT+ASA blend. It produces moldings with good surface finish, is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicati.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® A3EG7 35% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 35% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | IEC 1006 |
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs.. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3L PA6 (Conditioned) Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing. |
|||
Specific Heat Capacity | 1.50 J/g-°C | 0.359 BTU/lb-°F | |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |