Material Notes:
Eastman Amphora™ 3D polymer is a low-odor, styrene-free choice that was developed for 3D Printing applications. With Amphora, makers can create items that are more functional, durable, efficient, and attractive. Amphora complies with certain U.S. Food and Drug Administration (FDA) regulations for food contact applications.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Tensile Strength, Yield 50.0 MPa
7250 psi
ASTM D638
Elongation at Break 110 %
110 %
ASTM D638
Elongation at Yield 5 %
5 %
ASTM D638
Tensile Modulus 1.90 GPa
276 ksi
ASTM D638
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 0.930 J/cm

@Temperature 23.0 °C
1.74 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Manufacturer mentions clarity but does not quantify
Processing Properties Metric English Comments
Nozzle Temperature 245 °C
473 °F
Users viewing this material also viewed the following: