Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eagle Brass 1008 Low Carbon Steel, 1/2 Hardened

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer Eagle Brass Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 1008 Low Carbon Steel, 1/2 Hardened.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughness. As a standard grade, 1008 steel is used in many common, low-stress applications. Weldability and brazeability are excellent. Typical uses include infrared counter measure flare substrate, electronic parts carrier, low ohm etched heating element and conductor grid elements.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 7.86 g/cc
0.284 lb/in³
As Annealed
Mechanical Properties Metric English Comments
Tensile Strength 379 - 517 MPa
55000 - 75000 psi
Elongation at Break 4.0 - 16 %
4.0 - 16 %
in 2 inches
Tensile Modulus 200 GPa
29000 ksi
Thermal Properties Metric English Comments
CTE, linear 15.8 µm/m-°C

@Temperature 20.0 - 649 °C
8.80 µin/in-°F

@Temperature 68.0 - 1200 °F
Thermal Conductivity 36.0 W/m-K
250 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Iron, Fe >= 99.685 %
>= 99.685 %
Calculated as Balance
Manganese, Mn <= 0.15 %
<= 0.15 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Sulfur, S <= 0.035 %
<= 0.035 %
Users viewing this material also viewed the following: