EMS-Griltech Grilene® KE 170 CoPES Mono-Component Fusible Adhesive Fiber

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer EMS-Griltech
Trade Name Grilene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilene® KE 170 CoPES Mono-Component Fusible Adhesive Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Grilene KE 170 is the higher melting CoPES mono-component fusible adhesive fiber. It is used in compact dry-laid nonwoven.Data provided by EMS-Griltech.
Physical Properties Metric English Comments
Fiber Count 5.50 dtex
4.95 denier
Processing Properties Metric English Comments
Melt Temperature 165 - 175 °C
329 - 347 °F
Descriptive Properties Value Comments
Color Raw White
Luster Bright
Staple Length 60 mm