Processing Properties Metric English Comments
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable E 1400 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable E1330I Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable EC486 DA Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable JC837DB Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable L00221 Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable WJCK504L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Wire & Cable WR8180L Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding
The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle..
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R7543E Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R7545H Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R7661A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R7831A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R8180K Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 160 - 175 °C
320 - 347 °F
SABIC HP4023W Low Density Polyethylene for Blown Film
Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo..
Melt Temperature 160 - 175 °C
320 - 347 °F
blown film equipment
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating  (discontinued **)
7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio..
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R3792C Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R3792E Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
PolyOne Geon™ Vinyl Flexible R8206A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Melt Temperature 165 - 175 °C
329 - 347 °F
Lucobit Lucofin® 7410 HFFR EBA MDH Cable Sheathing
Lucofin® 7410 HFFR is a thermoplastic, halogen free flame retardant and low smoke compound for the insulation and/ or sheathing of cables. This grade is based on ethylene butyl acrylate (EBA) and..
Melt Temperature 125 - 175 °C
257 - 347 °F
blown film extrusion
DuPont Elvax® 3170 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins..
Melt Temperature 125 - 175 °C
257 - 347 °F
blown film extrusion
DuPont Elvax® 3170SHB Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Blown Film
18 wt% Vinyl Acetate.Elvax® 3170SHB is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene res..
Melt Temperature 160 - 175 °C
320 - 347 °F
blown film equipment
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion ..
Melt Temperature 150 - 175 °C
302 - 347 °F
Blown Film Coextrusion
DuPont™ Elvax® 3169Z Ethylene Vinyl Acetate
DuPont™ Elvax® 3169Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3..
Melt Temperature 165 - 175 °C
329 - 347 °F
EMS-Griltech Grilene® KE 170 CoPES Mono-Component Fusible Adhesive Fiber
Description: Grilene KE 170 is the higher melting CoPES mono-component fusible adhesive fiber. It is used in compact dry-laid nonwoven.Data provided by EMS-Griltech.
Melt Temperature 150 - 175 °C
302 - 347 °F
DuPont Elvax® 3128 Ethylene-Vinyl Acetate Copolymer Resin for Blown Film  (discontinued **)
8.9 wt% Vinyl Acetate.Elvax® 3128 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resin..