Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Dymax 912 Strain Relief, Wire and Parts Tacking Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 912 Strain Relief, Wire and Parts Tacking Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 912 Strain Relief, Wire and Parts Tacking AdhesiveFast curing, withstands wave soldering while resisting most solvent and aqueous washes Cure Type: UV
Physical Properties Metric English Comments
Viscosity 26000 cP
26000 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 10.3 MPa
1500 psi
Processing Properties Metric English Comments
Cure Time <= 0.0833 min
<= 0.00139 hour
Descriptive Properties Value Comments
Cure Depth 0.25 in.