Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oceanchem Group Tris (2-chloroisopropyl) Phosphate (TCPP)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Oceanchem Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oceanchem Group Tris (2-chloroisopropyl) Phosphate (TCPP).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molecular Formula: C9H18O4Cl13PCas No.: 13674-84-5Property: It is colorless transparent oily liquid. Soluble in ethanol and chloroform, insoluble in aliphatic hydrocarbon, water solubility is less than 1%.Use: It is mainly used as soft or hard polyurethane foam, epoxy resin polystyrene, acrylic acid, cellulose acetate, ethyl cellulose paint, phenolic plastics, polyvinyl acetate and foam leak sealing agent. It has good heat conductivity and hydrolysis stabilizer, especially suitable for ASTME84 (grade). Its products have low viscosity in low temperature when it is used in polyurethane foam, unsaturated polyester and phenolic plastic.Storage and Packing: 250kg in galvanizing pail, storage temperature 5-38°C, in dry air, common chemicals.Information Provided by Oceanchem Group
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc

@Temperature 20.0 °C
1.29 g/cc

@Temperature 68.0 °F
Molecular Weight 327.4 g/mol
327.4 g/mol
Thermal Properties Metric English Comments
Flash Point 220 °C
428 °F
open
Optical Properties Metric English Comments
Refractive Index 1.46 - 1.466
1.46 - 1.466
n20D1
Component Elements Properties Metric English Comments
Chlorine, Cl 32.5 %
32.5 %
Phosphorous, P 9.46 %
9.46 %
Processing Properties Metric English Comments
Moisture Content <= 0.080 %
<= 0.080 %
Descriptive Properties Value Comments
Acidity <0.05
mg KOH/g
Appearance Colorless or light yellow oily transparent liquid
CAS Number 13674-84-5
Chroma 50
Pt-Co
Molecular Formula C9H18O4Cl13P
Users viewing this material also viewed the following: