Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 943 Polyester Film

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 943 Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 943 is a super clear film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 96.5 MPa
14000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 96.5 MPa
14000 psi
ASTM D882A
Film Elongation at Break, MD 200 %
200 %
ASTM D882A
Film Elongation at Break, TD 120 %
120 %
ASTM D882A
Coefficient of Friction, Dynamic 0.50
0.50
A-B; ASTM D1894
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
Film Tensile Strength at Break, TD 207 MPa
30000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.7 %

@Temperature 190 °C,
Time 300 sec
1.7 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 1.9 %

@Temperature 190 °C,
Time 300 sec
1.9 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Optical Density 0.69

@Thickness 0.127 mm
0.69

@Thickness 0.00500 in
ASTM D1003
0.69

@Thickness 0.178 mm
0.69

@Thickness 0.00700 in
ASTM D1003
0.69

@Thickness 0.254 mm
0.69

@Thickness 0.0100 in
Reference Wratten 18A Filter
Haze 0.40 %

@Thickness 0.127 mm
0.40 %

@Thickness 0.00500 in
ASTM D1003
0.50 %

@Thickness 0.178 mm
0.50 %

@Thickness 0.00700 in
ASTM D1003
1.0 %

@Thickness 0.254 mm
1.0 %

@Thickness 0.0100 in
ASTM D1003
Users viewing this material also viewed the following: