Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Film Tensile Strength at Break, MD = 24000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® 342 Polyester Film
Melinex® 342 is a two-side heat-sealable, clear polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well as a vari..
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® 561 Polyester Film
Melinex® 561 is a high clarity polyester film which is pretreated on both sides to promote adhesion to many industrial coatings and inks. Melinex® 561 is suitable for applications which require a ..
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® 725 Polyester Film
Melinex® 725 is a high clarity polyester film pretreated on both sides to promote adhesion to many industrial coatings and inks. Melinex® 725 exhibits improved performance in multi-pass printing a..
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® 965 Polyester Film, 500 Gauge
Melinex® 965 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by..
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® 966 Polyester Film, 700 Gauge
Melinex® 966 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by..
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Mylar® EC Polyester Film, 300 Gauge
Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta..
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Mylar® EC Polyester Film, 400 Gauge
Mylar® EC films are electrical grade films designed for use in applications where improved dimensional stability is required. In addition to lower levels of shrinkage, Mylar® EC films offer outsta..
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
DuPont Teijin Films Melinex® 943 Polyester Film
Melinex® 943 is a super clear film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems.Information provided by DuPont.