Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Neoprene GW Polychloroprene

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Neoprene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Neoprene GW Polychloroprene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Neoprene GW is a sulfur-modified polychloroprene stabilized with a thiuram disulfide. The crystallization rate of Neoprene GW is slightly faster than that of Neoprene GRT. Compounds of Neoprene GW cured with metal oxides alone have excellent processing safety, yet cure rapidly. Although not required, cure accelerators can be used and are advantageous for some applications. Properly compounded vulcanizates of Neoprene GW have high resilience and excellent flex cracking resistance, and the best tear strength of any type of Neoprene. Among the G types, vulcanizates of Neoprene GW are characterized by exceptionally good retention of properties after heat-aging. Compression set resistance is significantly improved over that of other G types, although it is not as good as that of thiourea-cured W types. Neoprene GW breaks down, or softens, to a lesser degree than other G types. compounds based on Neoprene GW will therefore exhibit a higher viscosity than similarly loaded compounds based on Neoprene GNA or GRT. Because of the higher compound viscosity, stocks based on Neoprene GW are slightly less sticky and have slightly less building tack than stocks based on other G types. Compounds of Neoprene GW have approximately the same viscosity as do similarly loaded compounds of Neoprene W.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D7920-66
Mooney Viscosity 37 - 49

@Temperature 100 °C
37 - 49

@Temperature 212 °F
ML (1+10); ASTM D1646-81
Descriptive Properties Value Comments
Color Light amber
Crystallization Rate Slow
Form Chips
Odor Mild, characteristic
Storage Stability Good
May undergo viscosity changes. Store under cool conditions and keep storage to a minimum.